You have to have access to this pipe to get it shot. I would also advise the following:
*That you look closely at the governing codes being that it's diesel.
*Pay attention to your spec, and looking into the grade of material being used.
*Look into the need for bitumen protection, this should be in conjunction with the assessment of the concrete encasement as well. In short, you need a corrosion analysis. I suspect you'll find this is a big one. If your specs don't have it covered, I suggest you get it covered as you don't want to be digging this up in 5 years on your dime.
Getting it radiographed before it goes into the ground will be the easy part.
Regards,
Gerald