Wrong! What I am referring to is what the Original Poster wrote since he should know first hand the test conditions and he wrote: Quote:
"Gents,
ISO 13847 is not a construction code it says all about qualification of WPS , NDT, DT as well as production weld.
Test temperature is -31°C
specimen size as per ASTM A370, notch depth 2 mm form the root
Test results of 1 set ( 3 specimens) : 13, 20 & 21 (required is minimum average 41.64, individual 29.64J)
'Cut it' means , he removed the complete weld deposition and rewelded it.
Thanks in advance
nand7400"
This is what I'm referring to Billy! Now would you please go get your eyes checked out already!
Henry