just walked in the door. worked 12 hrs through the nite, in the cold (north dakota) and snow, showed up on location waited 3hrs, finally cement was done , measured the spool, made it and then they wanted a flow line changed. totally different flange and pipe dia, but made it work did all that . Had to wake the company up at 10am sunday and man did i get an ass chewing for waking him up. i charged them 127.00 an hr plus consumables and mileage and helper, never had a problem before with this guy, i am freaked out because the we have a another huge job in the shop for the same company, and i wonder if we will lose it.. maybe im worrying to much i don't know...