- - By jaws (*) Date 12-29-2009 11:38
Hi All,

For suggested UT report form I could not find any report form in D1.1M. I found, but there is a not that mention this form can not be used for tubular structures. I am using D1.1M 2008 edition. this form is on page 344 Annex-M. Is there a ny suggested format for tubular structures or what type of report should I use.

Thanks
Parent - By jwright650 (*****) Date 01-04-2010 16:43
Your Level III has most likely included a form to use to report your examinations if he/she wrote a procedure for tubular UT examinations(per AWS D1.1:2008 para 6.27.1). You may have to contact the Level III and ask for a form to report your examinations on, if they did not include an example for you in the procedure.
Up Topic American Welding Society Services / Technical Standards & Publications / UT inspection

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill