Can anyone give me some tips other that what I have here on running this rod any help would be appreciated
HARRIS 26
Aluminum electrode featuring a precise combination of core wire and a unique extruded coating. Harris 26 provides a high speed deposition with dense, machinable welds. It is widely used on sheets, tubes and extrusions for thicknesses of 1/8” or more. Also suited to torch applications.
Procedure:
Clean weld area
Bevel sections greater than 1/4”
Preheat - 500°F is recommended on sections greater than 1/8”
DC-reverse polarity
Hold electrode in a vertical position
Remove flux between passes
Clean with hot water; add 10% sulphuric acid to water if additional cleaning is required
Features:
Tensile strength - Up to 34,000 psi
Good color match
Good corrosion resistance
Good electrical condutivity
Machinable
All position