- - By david bean (**) Date 01-22-2010 16:33
ASTM A513 is not shown in D1.1, Our auditor is requesting Qualified procedures for this. I have this in .095 and .120.

could i Qualify it to D1.3?

Any recommendations would be appreciated.

thanks,
David
Parent - By welderbrent (*****) Date 01-23-2010 17:03
David,

While D1.1 goes down to .120, D1.3 goes up to 3/16".  I would think that would work better for you so both are covered by one code.  JMHO.

I'm afraid that I'm not familiar with 513 off the top of my head and don't have ref books handy right now.  As long as other parameters are met it should be able to be done with a PQR.  Is that what you were looking for?  What process are you using?  What type of work is this for?

Just a couple of questions that come to my mind.  Otherwise, just my two tin pennies worth.

Have a Great Day,  Brent