- - By weaver (***) Date 03-03-2010 18:33
Anyone ever built a gas buster before? I might have a contract to build five or so.
Parent - - By 803056 (*****) Date 03-03-2010 20:39
A what?

Al
Parent - - By Stephen32 (*) Date 03-03-2010 22:40
Yep. Built many of them. AKA "Poor boy degasser".
Parent - - By weaver (***) Date 03-04-2010 00:14
can i pick your brain?. and i know knowledge is always worth something..
Parent - - By 803056 (*****) Date 03-04-2010 02:02
See, you never know. I was thinking along the lines of "Beano".

Best regards - Al
Parent - By welder81 (*) Date 03-04-2010 03:06
I have built a bunch of them from 48'' to 72'' ....
Parent - - By raftergwelding (*****) Date 03-04-2010 03:39
I've run the piping and hooked them up but never built a new 1
Parent - - By Stephen32 (*) Date 03-05-2010 17:54
Sure. What do you need? I was just going through old pictures looking at some of them.
Parent - By weaver (***) Date 03-05-2010 23:04
the internals, vessel size.  im sure it changes with the customer.  anything you could spare.  to be honest with you i don't know alot about them.. just being honest
Parent - - By Cactusthewelder (*****) Date 03-06-2010 01:07
Matt,
You still hangin in there ? When you gonna get back in your truck ?
Parent - - By raftergwelding (*****) Date 03-06-2010 15:11
You mean the El Camino?
Parent - - By Cactusthewelder (*****) Date 03-06-2010 16:00
YEP ! THATS THE ONE.............WITH THE HOBART
Parent - - By weaver (***) Date 03-06-2010 16:53 Edited 03-06-2010 18:15
you guys CANT be serious, a "welder" showed up to a job in an el camino with a hobart machine.. thats awesome.  we all have to start somewhere.
Parent - - By Cactusthewelder (*****) Date 03-06-2010 18:53
Sure did ! Stephen32. And he still has it ! He even has those Lowrider Hydraulics on it
Parent - By weaver (***) Date 03-06-2010 23:40
thats even more awesome!.  i love "out of the norm"  sweet..  matt do you have any pics ?
Parent - By raftergwelding (*****) Date 03-07-2010 20:40
To bad them low life thugs stole the spinner rims he had on it i wonder if its still sittin on blocks in the driveway
Parent - - By DaveBoyer (*****) Date 03-07-2010 04:42
Do You still have that picture of the Subaru Brat with the welder in the back?
Parent - - By raftergwelding (*****) Date 03-07-2010 20:39
now i dont it was posted on here some whee but that was a long time ago.
Parent - - By Stephen32 (*) Date 03-08-2010 21:20
Sorry guys internet has been down all day and was busy all weekend. Im about ready to get back out there. El Camino is still on blocks. Sold the brown Ford and bought a white 4 door Ford. Need to get it rigged out. Probably just leave the bed on it and work out of the back.

As far as starting out with the El Camino.... I had to work up to getting that one...
Parent - - By raftergwelding (*****) Date 03-09-2010 03:43
remember the time you sat on the hydraulics control and dumped all your equipment right there in the yard to bad i didnt have a camera lol
Parent - - By Stephen32 (*) Date 03-09-2010 14:20
That was a bad day.
Parent - - By raftergwelding (*****) Date 03-09-2010 21:46
at least the hobart didnt get all beat up.
Parent - - By slagline 3 (**) Date 03-10-2010 21:24
Weaver, I sent a private message.
Parent - By Stephen32 (*) Date 03-11-2010 21:46