I have an upcoming series of tests for an Inconel procedure development effort and am thinking about grinding consumables. Are there any grinding consumables that are a definite no-no because they leave junk in the ground surface? And likewise, are the grinding consumables that are more preferred because they are clean? I do not expect to be doing much grinding, so consumable longevity is not a big concern, it's more cleanliness I'm interested in.