- - By Inspector 1959 Date 04-15-2010 03:32
Our company purchased another company and now I need to know if we need to retest the welders, we use D1.1 and I can't find a clear answer.
Parent - - By 803056 (*****) Date 04-15-2010 15:27
There should be no reason to requalify the welders as long as the new owner accepts responsibility for the documentation provided by the old company. That can be accomplished with a signature of the person given that authority by the new owner.

If there is any question about the ability of the welders to meet the new owner's expectations, retest them.

Best regards - Al
Parent - By jsdwelder (***) Date 04-23-2010 12:16
In 2006 D1.1, 4.1.2.1 addresses this. I know 2006 is not the most current edition but I'm sure the '08 or '10 edition covers it as well.