Hello i want to weld 2 sheets of ultrafine grained aluminium (produced by ARB process) by cold roll bonding and test the residual stress in the weld zone. can you help me about the ways of measure the residual stress (except XRD) ? can anyone help me about the ABACUS software ? thanks
The only way I know to measure residual stress is by X ray difractometry. Is there any other? Is Abacus software used to measure residual stress after welding? If so, I'd also wish to know about it. Giovanni S. Crisi Sao Paulo - Brazil
This paper describes the use of a combination of XRD (X-Ray Diffraction) and mechanical (strain gage) techniques in order to measure residual stresses resulting from the fabrication process of Alloy 600 nozzle and heater sleeve mock-ups: