Date 05-13-2010 17:29
Went there found 50 or so, none seem to get me where I need to be.
I am looking to use a standard tried and true WPS Traceable to AWS D1.1 to qualify our welders to. Was hoping to find 2 actualy.
Material: M-1 Group1 and II The more flexible the better
Thickness: 1/8" to unlimited (Plate is all we need for now)
Joints: Groove, fillet, the more the better.
Processes: GMAW and GMAW-S
Shielding Gas: 98% Argon/2% Oxygen for the GMAW-spray
75% Argon/25% Co2 for the short Arc
Filler Metal ER70S-6
Filler Metal Dia. .035, .045 (1/16 and .020" would be nice)