Dear Friends I need to qualify PQR for 6-Moly x Carbon Steel Deck Penetration Doubler Plate-Fillet Weld Weld Process - SMAW or GTAW. Appreciate advise on suitable consumable and weld parameteres. Thanks
Which 6 MO? It matters since 6 Mo's are not all the same P-No. AL6XN happens to be P45. Some, like 254 SMO are P8. I suppose we would need a Section IX historian to explain why.