What material is the frame made from?
How are the tube end fittingss attached?
Do You have dissimilar metals where the corosion is taking place?
If so, they are causing a galvanic cell, which greatly accelerates corosion.
Dissimilar metals need to be electricly insulated from each other, or sealed from salt water/salt air or any electrolite.