Agree. The bend test will tell you if your weld technique is working; no cracks means no breakage. Also your chemistry and of course ductility of the weld and HAZ. However it will not indicate how strong the weld is. For that you have to pull tensiles. In addition to D1.2, check out B4.0 for mechanical test experiments.