Up Topic American Welding Society Services / Certifications / GTAW 6G with backing
- - By greek (*) Date 08-02-2010 16:58
Is this Prequalified in D1.1?
Parent - By jwright650 (*****) Date 08-02-2010 17:11
GTAW is not a pre-qualified process. See AWS D1.1:2010 Clause 3.2.2 Code Approved Processes.
Parent - By waccobird (****) Date 08-02-2010 17:13
greek
No
Good Luck
Marshall