Most of the job is A572, but there are a couple of stainless sequences. One of them is c-276 stainless, the other is duplex 2205 stainless, and both may have A992 or A588 in the mix. I haven't seen the drawings yet, as they are on hold with the EOR. I just want to get all my ducks in a row before the work hits, so if we do need to qualify welders, we are ready. The work is actually duct work for a power plant. I'm just not sure if I need to test the welders on c-276 to c-276, 2205 to 2205, c-276 to A992, c-276 to A588, etc., or does one weld test per D1.6 cover all?