- - By mike wiebe 3 (*) Date 08-13-2010 15:54
Anybody know if inconel 625 weld wire will be combatible to use on inconel 601?  First place was here to start my search, thanks.
Parent - - By MMyers (**) Date 08-13-2010 16:20
625 is not listed in the data sheet as a recommended consumable.  Recommended consumables are dependent on application and welding process.  See page 14 of the data sheet: http://www.specialmetals.com/documents/Inconel%20alloy%20601.pdf
Parent - By mike wiebe 3 (*) Date 08-13-2010 16:37
Excellent site! Thanks again.