Now I am unsure of your question!
A PWHT is an Essential Variable in a WPS for the purpose of STRESS RELIEF (residual welding stress's) primarily. What you discribe is not necessarly the same thing and yes it requires some experience.
So does the PWHT for that matter.
You need to understand the difference between STRESS RELIEF and HEAT TREAT.
Aligning joints does not necessarly require heat, if you are indeed working with High Strength material and you starting heating and bending then you will most likely need a HEAT TREAT to restore the required condition of the material.
In its simplest terms a Stress relief will never exceed the Tempering temperature of the base material.