Eutectic,
Interpretation: IX-83-143
Subject: Section IX, QW-351
Date Issued: November 26, 1984
File: BC84-58 1
Question: Can weld reinforcement be considered for determining the deposited weld metal
thickness per QW-351, provided that the full weld reinforcement is included in either the side bend
tests (where side bends are permitted by QW-452) or the radiographic examination (where permitted
by QW-30411
Reply: No,
Hope that helps,
Regards,
Shane