Yeah, that's the sure way to get it done.
The thing about complete welding in one pass is it halves the labor cost.
It just takes good operators who know what they're doing, and someone watching the inside, ready to shut down the SAW, in case of trouble.
If you hand weld the root from the inside, I suggest MCAW.
Tim