If Your rosebud is too large for the cylinder output, the pressure will drop off as You are working, and give You problems. Look up the CFM of the rosebud then figure the available gas delivery of Your tank using the 1/7 rule which is now the 1/10 or 1/15 rule. You probably have too large a rosebud for the cylinder.
See this thread:
http://www.aws.org/cgi-bin/mwf/topic_show.pl?tid=26905Propane or propalene will have the same problems if You draw hard enough on a small tank, but not nearly as bad as with acetylene.
Check the specifications on Your rosebud, many are fuel specific, You may need a different one for propane.