Hi Brian, Hi Chet,
Yes, Brian you're right I didn't spell it out far enough....
....[it should have read B-U2a-(G) or (F).
Guys, I would rather see the 3/8" groove filled in at least three passes too, but I was just figuring for arguement sake. Mathius' teacher wanted to see it done in two passes, so I was looking at this from other angles to see if it were possible by code. Look back at that Table 3.7 and in the column above Max Fill pass, there is a column for Max Root pass which says in the flat position under GMAW/FCAW [3/8"] and under the vertical postion w/ GMAW/FCAW [1/2"]. Then there's the note#4 which directs you back to the para 3.7.2.
So, If you were to fill this groove in one pass wouldn't that qualify as a root pass?
John Wright
PS, I figured it might not get seen, so I just restarted the question over because it would get lost in all those posts over on the other board.