I have a gentleman in my area who has a 1993 BobCat 225, with 613 hours on it, always serviced etc. The story I get is he was welding with it one day, cold in his shop, didn'nt think aircompressor was plugged in, then all of a sudden the air compressor comes on, his arch goes way down and hears a buzzing noise. Now, He says the 16 HP Onan enfine runs fine, but no welding output, generator doen't work. He feels he overloaded it, Has asked around and been told that on older Miller generators when they go out it is almost impossible to get parts and not worth trying to fix. He bought another welder, and wants to sell the Bobcat cheap. Anybody familiar with this type of BobCat problem? Worth trying to fix, Parts? I really value all your advice.
Thanks
Dave in Iowa