I have a pipe bendrer from HF, it bends pipe OK, but it might not make a nice bernd in thin walled tubes. The inside dies are sized for Sch. water pipe, the outside is just rollers with a large radius groove. You probably need a Hosfeld or similar with the proper tooling. Find someone that has one & will work with You.