I didn't see any provision in D1.1-2010 allowing the evaluation of a welder performance test coupon using UT. There is a provision that permits the use of RT in lieu of performing the guided bend test.
Best regards - Al
While many welds are examined by the UT method I don't see any indication of acceptance for UT in place of RT or Bend Tests for Welder Qualification. Not in D1.1 anyway.
While away from my computer I see Al beat me to an answer.
Have a Great Day, Brent
it is permitted according to ASME SEC IX 2010 QW 302.2 not AWS D1.1
regards