Save yourself some money and buy E312 (if that is what you need) from one of the major manufacturers instead of the "magic rod" vendors. Their "super missile weld" names or rainbow colored coatings are all for show to make you think you're getting something special. Also, as you can see from Shane's post, the carbon content is quite high for E312 compared to other SS alloys.