- - By Tyler1970 (***) Date 03-08-2011 00:42
I was just wanting to see some dowhill caps. And what are your techniques. thanks
Parent - - By hillbilly delux (***) Date 03-08-2011 11:28
lower your amperage and weave from one side of the bevel to the other keeping your rod angle always below your puddle as to push it up. pretty simple really. Hard part is mastering just that.
Parent - - By Tyler1970 (***) Date 03-08-2011 21:20
i was just wanting to see other caps.
Parent - - By hillbilly delux (***) Date 03-09-2011 01:07
Will take some tomarrow
Parent - - By Tyler1970 (***) Date 03-09-2011 01:31
here is mine. 18 in .375 3/16 70+ and a 8 in .375 3/16 70+
Parent - - By welderbrent (*****) Date 03-09-2011 03:32
Tyler,

Though the pic was a bit blurry, those look pretty good. 

You just wanting to compare yourself with others, or is there something in particular you are looking for? 

Have a Great Day,  Brent
Parent - By Tyler1970 (***) Date 03-09-2011 05:09
Im trying to find some of the best looking caps so I can improve. I find the cap puts the finishing touch on a weld.
Parent - By texasrigwelder (**) Date 03-09-2011 01:18 Edited 03-09-2011 02:08
6 inch 500 wall arkansa bellhole part of chesapeak test.  Was my reup


Bastard side
Parent - - By Blaster (***) Date 03-09-2011 01:23
I like a slight drag with a slight side to side until getting to the bottom.  Coming into the bottom I like to work into a slight push, going into either circles or a minor whip with the electrode.
Parent - - By Pickupman (***) Date 03-09-2011 01:56
I wish mine looked that nice Tyler. The bottom is still kickin my tail with 3/16, but getting more consistent.
Parent - By Tyler1970 (***) Date 03-09-2011 04:14
im get a pic of the bootom tomorrow.
Parent - - By ibeweldingsum (***) Date 03-12-2011 01:50
heres a pic of one i did a couple of days ago
Parent - By Tyler1970 (***) Date 03-12-2011 04:39
that pics super small on my comp. but what i can make out its slick.