Thank you all for your replies, and thank you Brent, I gleened a ton of info from that source.
What I'm referring too, the company I work for has been burned because a supplier of a major component, has assembled it with couterfeit bolts, origin Red China. These bolts are stamped, came with CMTR's, metallurgy, everything, but the documantation was false. Now, my company is stuck with the repair replacement, and the silly thing is, our purchasing gurus want to buy the replacement bolts from, where else, Red China. I was looking to avert that, and didnt have as much time as I would have liked to put together a persuasive argument.
The problem is solved now, and we are replacing with US made fasteners.