Is there anything in D17.1 that specifically requires you to use GTAW? Is it permissible to use GMAW with this spec?
By
Ringo
Date
03-10-2011 17:38
yes,its listed in section 5.
By
Lawrence
Date
03-10-2011 18:00
Zeek,
The *fusion* welding processes are listed in D17 Table 5.1
Please keep in mind the Procedure (PQR/WPS/Welder Performance) qualification requirements that go along with a change in process.
See 5.2.2.1
By
Zeek
Date
03-15-2011 18:13
Thanks. I completely missed it...it was in Table 4.1
Topic
Welding Industry
/
General Welding Discussion
/ AWD D17.1 GMAW?
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill