![](/mwf/attachments//avatars/6875-2101.jpg)
New to D17.1 and I need advise, suggestions to help me get things right.
I’ve come into a situation that I’ve found “D17.1” performance qualification records that indicate that the tests were to Class “C” requirements and I’ve not found any Welding Procedure Qualification Records to support the WPS’s referenced.
The way that I’m interpreting D17.1 it tells me that I’ll need to start testing over from scatch to get these jobs compliant to D17.1 .
"4.2.2 Qualification Requirements. To achieve qualified status, welders and welding operators shall demonstrate their skill by producing acceptable test welds per the requirements of
Paragraph 4.3.8. Test welds should not be required for those welds that will not be required inproduction welding. Qualifications, certifications, requalifications, and recertifications given under this document do not transfer from one fabricator to another."
Paragraph 4.3.8.1 inferrs that *All* welding performance testing will be done to inspection criteria for Class "A" welds, and class "A" welds require a procedure that is qualified by testing.
For
performance qualification to Class “A” the test need to meet VT Class “A” 6.3 and table 6.1,
and
PT/MT depending on if it is ferrous or nonferrous
and
RT.
Only after the
procedures are qualified D17.1 Paragraph 4.4.3 by testing to AWS B2.1
Then it will need
Visual (D17.1 tale 6.1 not the requirements of B2.1)
And
Guided bend test
and
And tensile testing
Help Please,