Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Technical Discussions / What's the difference of TP347HFG and TP347H?
- - By dragon (**) Date 03-02-2011 06:09
Dear all
I only get TP347HFG should  be cold finished from ASME II A.

ANY REPLY WILL BE APPRECIATED!

REGARDS FOR
LU
Parent - - By waccobird (****) Date 03-02-2011 10:11
dragon
Was waiting to go to work and saw your post.
Didn't have the slightest idea what you were referring to so I did a google search and found that the difference is  (TP347H is coarse grain ) and (TP347HFG (FG) Fine Grain)
http://books.google.com/books?id=vIwAuzWcKRAC&pg=PA444&lpg=PA444&dq=What's+the+difference+of+TP347HFG+and+TP347H%3F&source=bl&ots=HGPLAqSiKx&sig=ebW1Sbn6SeA_QAwFP39jDivnAfw&hl=en&ei=HBZuTf_DB9K9tgfKvsmGDw&sa=X&oi=book_result&ct=result&resnum=7&ved=0CDsQ6AEwBg#v=onepage&q&f=false
Good Luck
Marshall
Parent - - By dragon (**) Date 03-05-2011 02:55
waccobird,
Thank you very much!

The book  you searched is very useful for me!

What filler wire shoud be used for welding TP347HFG?
Parent - By playboy1898 (*) Date 03-31-2011 00:28
I think the ER347 is ok. 347H+347H the filler metal is 347.
You can see the AWS D1.6.
The chemical element and component of TP347HFG is the Same as TP347H(347H). Only the process of produce changed so that the Grain of the steel is changed.

Use TIG (GTAW) with small heat input.
The interpass Temp. not exceed 150℃.