Good morning guys,
We are having an issue welding 572 gr 65 to 316 ss plates using E810X - ni1- we are seeing centerline and toe cracking of some of the welds. Does anyone here have any sussgestions as to why this may be happening? Beyond the immediate - I believe that we need to change to a 309 FCAW wire, but I am still curious as to why the cracking would be happening with what we are using right now, and what steps could be done to negate the issue in the short term.