- - By HAFIZ USMAN IFTIKHAR Date 04-20-2011 11:20
can anyone guide me to avoid pits in argon welding of stainless steel/300/400 series
give me variety of reasons
Parent - By OBEWAN (***) Date 04-20-2011 11:41
Argon is not a welding process it is a welding shielding gas material and it has no concerns when welding with stainless.

You neeed to be more specific about the process to get an answer.  Are you asking about GMAW, GTAW, FCAW, PAW, SAW, or which process or all processes?