AWS A3.0
Welding Procedure Specification
A document providing the required welding variables for a specific application to assure repeatability by properly trained welders and welding operators.
Welding Procedure Qualification Record
A record of welding variables used to produce an acceptable test weldment and the results of tests conducted on the weldment to "qualify a welding procedure specification". (quotes mine)
Sounds pretty cut and dried to me.
Now I would submit (without degrading into some Clintonian semantics) that if you are faced with the idea of repeatability on a 'pre WPS' you ain't doing it right.
![wink :wink:](/f2/epx.png)
I sorta think the idea to a PQR is actually avoiding repeatability(which would be the case with a pre WPS as well of course). If you get it right or wrong why would you want to repeat?
And try as I might I just don't see 'pre WPS' in 3.0 anywheres at all at all.
![confused :confused:](/f2/epx.png)
But of course given the great sophistication of many operations (I myself may be just too backwoods to understand-why heck we's still weldin with them thar wood rods and I haven't been able to git mah still outa the shop) I can see the use for a Pre WPS. Though I would submit that even more sophisticated operations (maybe the Japanese) would wish to base their pre WPS on some solid mechanical testing basis in which case Pre PQR would be in order and they cna then laugh at us for our fingers in our noses. But then doesn't this smack of ad infinitum?
Which comes first? Cluck, cluck, cluck.
Fortunately the codes have settled it for us.