- - By Barbaros (*) Date 04-22-2011 11:26
On WPSs it is indicating that cap size as: 5-7 or BAB extended.

And the question is; what does BAB extended means?

Thanks.
Parent - - By weldwade (***) Date 04-22-2011 16:22
Now I have a question, cap size 5-7? The only caps I know of are back caps in short medium or long. I have heard nozzles referred to as "cups" and they would be sized in #5 or #7 etc. BAP extension??? I have no clue.
Parent - - By Barbaros (*) Date 04-23-2011 07:56
Sorry, typing error. The word is 'cup' of course.
Parent - - By fschweighardt (***) Date 04-24-2011 02:49
I think the size is diameter in eights, i dont know BAB, but they might be referring to a gas lens
Parent - By 522029 (***) Date 04-24-2011 11:20
They are sized in 1/16 ths.

Griff
Parent - By DaveBoyer (*****) Date 04-25-2011 02:05
I don't recall seeing the "BAB" designation, but there are long and short cups, at least in some sizes.