Hey Tim are you inspecting to D1.1?
If so, Table 6.1 (1) has pretty strong language concerning cracks.
...if it is incomplete fusion, Table 6.1(2) has specific language dealing with that also.
How are you determining the extent of the "indications of concern"? exploratory grinding? followed by MT?