I need to qualify a procedure to weld A216 to A572 Gr. 50 (CJP) and A216 to A53 std. pipe (Fillet) using E71-T8 (NR 232), I am not able to locate a plate of A216 for the procedure qualification. ASTM A216 is used extensively in pipe valves and other fittings, however we are using only a small saddle not large enough to test. Can anyone help me out?
Thank You,
Phillip Joe Jensen, AWS CWI #05061191, Hershberger Bros. Welding Inc., Las Vegas, Nevada
e-mail: joe@unionerectors.com