Thank you MBSims!
I have lost count of how many times i've been told by contractors "we don't need no stinkin' wps because all fillet welds are pre-qualified"...i just open to clause 3 under scope and ask them to read it and then i ask for their prequalified wps for fillet welds...it's like the 'circle of life'
and then when they discover that not "all fillet welds are prequalified"...well sounds like you've been there too...
Thanks again MBSims!
ziggy