Just compiling as many codes or standards that address deposited weld bead width.
Thank you Joey, that does apply but only to weld repairs to P1 Gr 1,2,3 and P3 Gr 1,2,3 matls..
And thanks, Doug for the D1.1 (2010) reference. Although 3.7.2 describes the limits, a welder really isn't limited to an electrode core diameter relationship to deposited weld bead width. I do see the reasoning behind limiting the size in Fig 1 as being stress factors in the T-joint configuration.
QCRobert