if somebody have some tips to spotweld galvalum with stainless
we have to weld 24 small projection in stainless steel on a sheet of galvalumn the machine is a press projection 600volts 300 kva the 24 projection hare on 6 different bracket and each of the upper electrode are hydraulic compensation  please send any idea
Parent - By OBEWAN (***) Date 10-14-2011 19:39
This should be posted in the resistance welding forum.