Try reading from A5.01:
4.2 Definitions. The terms dry batch, dry blend, wet mix, and heat, as they are defined and used in this document, refer to discrete quantities of the components used in producing a lot of filler metal. The definition of these terms and the considerations that must be given to the identification of the components to which they apply are as follows.
and also
5. Lot Classification