- - By toby250 Date 11-17-2011 12:22
Is this hard to weld,work with..whats the best welding procedure...is it anything like aluminium...i might have a job in the new year working with cunifer so trying to gather as much info as i can... thanks to anyone that can help :smile:
Parent - By welderbrent (*****) Date 11-17-2011 22:34
Never worked with it that I know of...but often, as Ravi said, you can find that documentation on the internet by Googling it.  Will give you all kinds of info.  Hopefully others here have actually used it and will pitch in.

Now, the reason I posted...

WELCOME TO THE AWS WELDING FORUM!!

Have a Great Day,  Brent
Parent - By ozniek (***) Date 11-18-2011 10:33
Hi toby250

Just make sure if it is cunifer, or CuNi. Some people in our part of the world incorrectly call CuNi cunifer. If you are going to take the trouble of studying how to do the welding, then best that you study the right thing!

Regards
Niekie
- By ravi theCobra (**) Date 11-17-2011 21:27
The material is Copper / Nickel / Iron  (Fe)

This material is well documented  in the  AMS  literature