I usually try to buy Excellene or Carol welding cable. I found a pretty good deal on some Flex O Prene. Anybody used it before? Is it worth a flip or just cheap?
Flex-A-Prene and Caroleprene both have EPDM jackets so they will wear about the same. The only difference seems to be the strand count of the copper. The Carolprene 2/0 has 1248 strands of 30 gauge while the Flex-A-Prene has 1235 strands of 30 gauge. I have had this cable for about a year and a half and so far so good.
I appreciate the replies. A spool of cable is a good chunk of $ that is hard to part with if you are unsure of the quality. I found a spool of 1/0 a guy will let go at $2 a foot!!