Oldie but goodie. 220 single phase. High frequency is out....it is either a cheap capacitor or the pot on the front...the coil checked good. Have burned 3/32-5/32 rods with it and it welded fine. $600. Will consider trades...good 2/0 lead, suitcase feeders...what do you got?