What is exactly the piece that has to be welded?
The dished end of a pressure vessel is made from a steel plate (hot rolled) that has been either pressed or spun (cold formed) to the desired shape, and can be perfectly welded.
So, you should clear up what's the piece you're talking about.
Giovanni S. Crisi
Sao Paulo - Brazil