![](/mwf/attachments//avatars/4269-2369.jpg)
If those wires will be used for different positions, then I would write seperate WPSs just to keep the confusion to a minimum.
I'm still wondering which wire that you have that shows E70T not being recommended for Horizontal welding. We've used ESAB, Hobart, and Lincoln FCAW E70T wires and all of them were Flat 1F,1G and Horizontal 2F, 2G. I regularly test our welders 2G unlimited with a E70T and rarely do I have any failures. We weld full-pen outriggers on columns and beams with that wire and that is all done in the 2G position. Full-pen stiffeners are all done in 2G...so that is why I'm wondering what wire mfg won't recommend their E70T in a 2G. We can turn/position all of our welding so that it is either Flat or Horz, so I don't even bother testing for anything else.
SAW wires tend to say Flat only, but that is due to the high currents and travel speeds of that process. Can you share what E70T, Flat only wire this is that you are using?