I think the question is not regarding two welders but one welder using two processes on the capping runs.
The way I read it the cap is made up of 3 runs - one run GTAW, two runs SMAW. (Why, I have no idea ?)
I cannot see any problem as long as all deposited weld metal variables have been complied with,
Regards,
Shane