These are not real aggressive tread, but I have been getting real good wear out of some Negotiator AT's on the back...running Hankook dynapro on the front (more of a street tread but stops good in the rain). I have had real bad luck with BFG AT's on anything with any weight to it...they all would separate in the summertime.