>Now, your flux is a separate issue. If you are getting the discontinuities because of the moisture in the flux I would think they would be anxious to remedy the situation.
How can a Discontinuity be ALWAYS tolerated if they MUST be repaired when they pass the Acceptable tolerances of the applicable code?
>Discontinuity; Break in normal physical structure
>Indication; Discontinuity of a size detectable to the examination medium, but below the recordable threshhold.
>Flaw; Indication that exceeds the minimum recordable size, but stays under the minimum rejectable size.
>Reject/Defect; A flaw that exceeds the maximum size deemed acceptable by the governing code/engineering specification.