hi all, someone supports me with their knowledge and affirms this, or is wrong.
I have 2 WPS
WPS "X" for welded joints under material specifications (group I) with (group I)
The following steps of welding electrodes that are listed:
Welding process process Filler metal
class - diameter
1 root SMAW E-6010 - 3/32”
SMAW E-6010 -1/8”
2 hot Step SMAW E-6010 -5/32”
3 filling SMAW E-7018 -1/8”
5/32”
4 view SMAW E-7018 -1/8”
I have this WPS qualified welders, AWS D1.1 allows me to apply these welders weld using WPS "Y"??
and
WPS "Y" for welded joints under material specifications (group II) with (group II)
The following steps of welding electrodes that are listed:
Welding process process Filler metal
class diameter
1 root SMAW E-7018 3/32”
2 hot Step SMAW E-7018 1/8”
3 filling SMAW E-7018 1/8”
4 filling SMAW E-7018 5/32”
5 view SMAW E-7018 1/8”
According to Table 4.12 of AWS D1.1 2006, understand that these welders must WPS requalify to "Y".
My interpretation is that correct?
really appreciate your assistance, rusbeli